{"title":"Joining Dissimilar Materials Using Three-Dimensional Electrodeposited Film","authors":"T. Kobayashi, K. Yamazaki, I. Shohji","doi":"10.23919/ICEP55381.2022.9795513","DOIUrl":null,"url":null,"abstract":"In this study, the effect of the shape of Ni-Cu alloy electrodeposited films, which was changed by using different concentrations of Ni amidosulfate in a plating bath, on the joint strength of stainless steel/CFRTP and aluminum alloy/CFRTP lap joint specimens was investigated. A lap joint specimen with the stainless steel and CFRTP joined using the Ni-Cu alloy electrodeposited film made of 450 g/L Ni amidosulfate showed an average joint strength of 18.4 MPa, which is higher than any of the other conditions. The average joint strength of the aluminum alloy/CFRTP ranged from 7 to 10 MPa.","PeriodicalId":413776,"journal":{"name":"2022 International Conference on Electronics Packaging (ICEP)","volume":"1 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2022-05-11","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"2022 International Conference on Electronics Packaging (ICEP)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.23919/ICEP55381.2022.9795513","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
In this study, the effect of the shape of Ni-Cu alloy electrodeposited films, which was changed by using different concentrations of Ni amidosulfate in a plating bath, on the joint strength of stainless steel/CFRTP and aluminum alloy/CFRTP lap joint specimens was investigated. A lap joint specimen with the stainless steel and CFRTP joined using the Ni-Cu alloy electrodeposited film made of 450 g/L Ni amidosulfate showed an average joint strength of 18.4 MPa, which is higher than any of the other conditions. The average joint strength of the aluminum alloy/CFRTP ranged from 7 to 10 MPa.