{"title":"Degradasi Zat Warna Indigosol Red Ir Menggunakan Metode Sonolisis Dengan Bantuan Katalis ZnO","authors":"Indah Humaira Saragih, Hary Sanjaya","doi":"10.24036/periodic.v12i2.117679","DOIUrl":null,"url":null,"abstract":"This research was conducted for the modeling degradation process of Indigosol Red Ir dye using the sonolysis method with the help of a ZnO catalyst. This study aims to determine the optimum mass addition of ZnO catalyst in the degradation process of Indigosol Red Ir dye. Sonolysis method using an ultrasound with frequency 47 kHz. The results of the percent degradation were seen from the absorbance measurement using a uv-vis spectrophotometer at a maximum wavelength of 510.2 nm. The results showed that the addition of the optimum mass of ZnO catalyst was 0.05 grams with a degradation percentage of 93.72%.","PeriodicalId":213875,"journal":{"name":"Jurnal Periodic Jurusan Kimia UNP","volume":"44 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2023-08-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Jurnal Periodic Jurusan Kimia UNP","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.24036/periodic.v12i2.117679","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 0
Abstract
This research was conducted for the modeling degradation process of Indigosol Red Ir dye using the sonolysis method with the help of a ZnO catalyst. This study aims to determine the optimum mass addition of ZnO catalyst in the degradation process of Indigosol Red Ir dye. Sonolysis method using an ultrasound with frequency 47 kHz. The results of the percent degradation were seen from the absorbance measurement using a uv-vis spectrophotometer at a maximum wavelength of 510.2 nm. The results showed that the addition of the optimum mass of ZnO catalyst was 0.05 grams with a degradation percentage of 93.72%.