{"title":"采用铜柱凸点作为第一次互连的45纳米极低k芯片的挑战","authors":"Po-Jen Cheng, C. Chung, T. Pai, D. Y. Chen","doi":"10.1109/ECTC.2010.5490768","DOIUrl":null,"url":null,"abstract":"In this study, Cu pillar bump is firstly built on FCCSP with 65 nm low k chip. 7 DOE cells are designed to evaluate the effects of Cu pillar height, Cu pillar diameter, PI opening size and PI material on package reliability performance. No obvious failure is found after package assembly and long-term reliability test. The packages are still in good shape even though the reliability test is expanded to 3x test durations With the experiences of Cu pillar bump on 65 nm low k chip, Cu pillar bump is again built on FCBGA package with 45 nm ELK chip. White bump defect is found after chip bond via CSAM inspection, failure analysis shows that the white bump phenomenon is due to crack occurs inside ELK layer. A local heating bond tool (thermal compression bond) is used to improve ELK crack, test results illustrate ELK crack still exists, however the failure rate reduces from original 30%~50% to 5%~20%. Simulation analysis is conducted to study the effect of PI opening size and UBM size on stress concentration at ELK layer. Small PI opening size can reduce stress distribution at ELK layer. On the contrary, relatively large PI opening size and large UBM size also show positive effect on ELK crack. Assembly process and reliability test are conducted again to validate simulation results, experiment data is consistent with simulation result.","PeriodicalId":429629,"journal":{"name":"2010 Proceedings 60th Electronic Components and Technology Conference (ECTC)","volume":"110 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"2010-06-01","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"13","resultStr":"{\"title\":\"A challenge of 45 nm extreme low-k chip using Cu pillar bump as 1st interconnection\",\"authors\":\"Po-Jen Cheng, C. Chung, T. Pai, D. Y. Chen\",\"doi\":\"10.1109/ECTC.2010.5490768\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"In this study, Cu pillar bump is firstly built on FCCSP with 65 nm low k chip. 7 DOE cells are designed to evaluate the effects of Cu pillar height, Cu pillar diameter, PI opening size and PI material on package reliability performance. No obvious failure is found after package assembly and long-term reliability test. The packages are still in good shape even though the reliability test is expanded to 3x test durations With the experiences of Cu pillar bump on 65 nm low k chip, Cu pillar bump is again built on FCBGA package with 45 nm ELK chip. White bump defect is found after chip bond via CSAM inspection, failure analysis shows that the white bump phenomenon is due to crack occurs inside ELK layer. A local heating bond tool (thermal compression bond) is used to improve ELK crack, test results illustrate ELK crack still exists, however the failure rate reduces from original 30%~50% to 5%~20%. Simulation analysis is conducted to study the effect of PI opening size and UBM size on stress concentration at ELK layer. Small PI opening size can reduce stress distribution at ELK layer. On the contrary, relatively large PI opening size and large UBM size also show positive effect on ELK crack. Assembly process and reliability test are conducted again to validate simulation results, experiment data is consistent with simulation result.\",\"PeriodicalId\":429629,\"journal\":{\"name\":\"2010 Proceedings 60th Electronic Components and Technology Conference (ECTC)\",\"volume\":\"110 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"2010-06-01\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"13\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"2010 Proceedings 60th Electronic Components and Technology Conference (ECTC)\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/ECTC.2010.5490768\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"2010 Proceedings 60th Electronic Components and Technology Conference (ECTC)","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/ECTC.2010.5490768","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 13

摘要

本研究首次在65 nm低k芯片的FCCSP上构建了铜柱凸点。设计了7个DOE电池,评估了铜柱高度、铜柱直径、PI开口尺寸和PI材料对封装可靠性性能的影响。经过封装组装和长期可靠性试验,未发现明显故障。虽然可靠性测试时间延长至原来的3倍,但封装仍然保持良好状态。在65纳米低k芯片上的铜柱凸点的经验基础上,采用45纳米ELK芯片的FCBGA封装再次构建了铜柱凸点。通过CSAM检测发现贴片粘结后出现白色凸起缺陷,失效分析表明白色凸起现象是由于ELK层内部出现裂纹所致。采用局部加热粘结工具(热压粘结)对ELK裂纹进行了改善,试验结果表明ELK裂纹仍然存在,但故障率由原来的30%~50%降低到5%~20%。模拟分析了PI开孔尺寸和UBM尺寸对ELK层应力集中的影响。较小的PI开口尺寸可以减小ELK层的应力分布。相反,较大的PI开孔尺寸和较大的UBM尺寸对ELK裂纹也有积极的影响。再次进行了装配工艺和可靠性试验,验证了仿真结果,实验数据与仿真结果一致。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
A challenge of 45 nm extreme low-k chip using Cu pillar bump as 1st interconnection
In this study, Cu pillar bump is firstly built on FCCSP with 65 nm low k chip. 7 DOE cells are designed to evaluate the effects of Cu pillar height, Cu pillar diameter, PI opening size and PI material on package reliability performance. No obvious failure is found after package assembly and long-term reliability test. The packages are still in good shape even though the reliability test is expanded to 3x test durations With the experiences of Cu pillar bump on 65 nm low k chip, Cu pillar bump is again built on FCBGA package with 45 nm ELK chip. White bump defect is found after chip bond via CSAM inspection, failure analysis shows that the white bump phenomenon is due to crack occurs inside ELK layer. A local heating bond tool (thermal compression bond) is used to improve ELK crack, test results illustrate ELK crack still exists, however the failure rate reduces from original 30%~50% to 5%~20%. Simulation analysis is conducted to study the effect of PI opening size and UBM size on stress concentration at ELK layer. Small PI opening size can reduce stress distribution at ELK layer. On the contrary, relatively large PI opening size and large UBM size also show positive effect on ELK crack. Assembly process and reliability test are conducted again to validate simulation results, experiment data is consistent with simulation result.
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Development of CMOS-process-compatible interconnect technology for 3D-stacking of NAND flash memory chips Inductance properties of silicon-in-grown horizontal carbon nanotubes Direct chip powering and enhancement of proximity communication through Anisotropic Conductive adhesive chip-to-chip bonding Cost comparison for flip chip, gold wire bond, and copper wire bond packaging An investigation of reliability and solder joint microstructure evolution of select Pb-free FCBGA pad finish and solder ball alloy combinations
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1