{"title":"SOI在高温运行中的优势论证","authors":"W. Krull, J.C. Lee","doi":"10.1109/SOI.1988.95439","DOIUrl":null,"url":null,"abstract":"Summary form only given. To evaluate the performance of SOI circuits at high temperatures, CMOS 4K SRAMs were fabricated on SIMOX (separation by implantation of oxygen) and bulk starting material. Four varieties were included in this study: bulk (5 mu m epi on n/sup +/), and SIMOX/SOI with three silicon-layer thicknesses (0.5 mu m, 0.75 mu m, and 1.0 mu m). This combination allows the assessment of three device structures: standard bulk devices, standard SOI devices (S/D contacting the buried oxide), and semi-bulk SOI devices which operate like bulk devices but are dielectrically isolated. All the SOI SRAMs were functional to the maximum temperature available, 300 degrees C. The bulk circuits also functioned at elevated temperatures, but lost functionality between 250 degrees C and 275 degrees C due to the rapidly increasing leakage current associated with the well junction. The synchronous access time increased approximately linearly with temperature for all devices, and was nearly twice the measured room-temperature value at 300 degrees C. Leakage current increased strongly with temperature for all devices, with the thin SOI devices having the least static current at the highest temperatures.<<ETX>>","PeriodicalId":391934,"journal":{"name":"Proceedings. SOS/SOI Technology Workshop","volume":"1 1","pages":"0"},"PeriodicalIF":0.0000,"publicationDate":"1988-10-03","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"24","resultStr":"{\"title\":\"Demonstration of the benefits of SOI for high temperature operation\",\"authors\":\"W. Krull, J.C. Lee\",\"doi\":\"10.1109/SOI.1988.95439\",\"DOIUrl\":null,\"url\":null,\"abstract\":\"Summary form only given. To evaluate the performance of SOI circuits at high temperatures, CMOS 4K SRAMs were fabricated on SIMOX (separation by implantation of oxygen) and bulk starting material. Four varieties were included in this study: bulk (5 mu m epi on n/sup +/), and SIMOX/SOI with three silicon-layer thicknesses (0.5 mu m, 0.75 mu m, and 1.0 mu m). This combination allows the assessment of three device structures: standard bulk devices, standard SOI devices (S/D contacting the buried oxide), and semi-bulk SOI devices which operate like bulk devices but are dielectrically isolated. All the SOI SRAMs were functional to the maximum temperature available, 300 degrees C. The bulk circuits also functioned at elevated temperatures, but lost functionality between 250 degrees C and 275 degrees C due to the rapidly increasing leakage current associated with the well junction. The synchronous access time increased approximately linearly with temperature for all devices, and was nearly twice the measured room-temperature value at 300 degrees C. Leakage current increased strongly with temperature for all devices, with the thin SOI devices having the least static current at the highest temperatures.<<ETX>>\",\"PeriodicalId\":391934,\"journal\":{\"name\":\"Proceedings. SOS/SOI Technology Workshop\",\"volume\":\"1 1\",\"pages\":\"0\"},\"PeriodicalIF\":0.0000,\"publicationDate\":\"1988-10-03\",\"publicationTypes\":\"Journal Article\",\"fieldsOfStudy\":null,\"isOpenAccess\":false,\"openAccessPdf\":\"\",\"citationCount\":\"24\",\"resultStr\":null,\"platform\":\"Semanticscholar\",\"paperid\":null,\"PeriodicalName\":\"Proceedings. SOS/SOI Technology Workshop\",\"FirstCategoryId\":\"1085\",\"ListUrlMain\":\"https://doi.org/10.1109/SOI.1988.95439\",\"RegionNum\":0,\"RegionCategory\":null,\"ArticlePicture\":[],\"TitleCN\":null,\"AbstractTextCN\":null,\"PMCID\":null,\"EPubDate\":\"\",\"PubModel\":\"\",\"JCR\":\"\",\"JCRName\":\"\",\"Score\":null,\"Total\":0}","platform":"Semanticscholar","paperid":null,"PeriodicalName":"Proceedings. SOS/SOI Technology Workshop","FirstCategoryId":"1085","ListUrlMain":"https://doi.org/10.1109/SOI.1988.95439","RegionNum":0,"RegionCategory":null,"ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"","JCRName":"","Score":null,"Total":0}
引用次数: 24

摘要

只提供摘要形式。为了评估SOI电路在高温下的性能,采用SIMOX(氧注入分离)和块状起始材料制备了CMOS 4K sram。本研究包括四种品种:块状(n/sup +/上5 μ m epi)和SIMOX/SOI,具有三种硅层厚度(0.5 μ m, 0.75 μ m和1.0 μ m)。这种组合可以评估三种器件结构:标准块状器件,标准SOI器件(S/D与埋地氧化物接触),半块状SOI器件与块状器件一样工作,但介质隔离。所有SOI sram都能在最高可用温度300℃下工作,整体电路也能在高温下工作,但在250℃至275℃之间,由于与井结相关的泄漏电流迅速增加而失去功能。所有器件的同步存取时间都随温度近似线性增加,在300℃时几乎是室温测量值的两倍。所有器件的泄漏电流都随温度的升高而强烈增加,在最高温度下,薄SOI器件的静态电流最小。
本文章由计算机程序翻译,如有差异,请以英文原文为准。
查看原文
分享 分享
微信好友 朋友圈 QQ好友 复制链接
本刊更多论文
Demonstration of the benefits of SOI for high temperature operation
Summary form only given. To evaluate the performance of SOI circuits at high temperatures, CMOS 4K SRAMs were fabricated on SIMOX (separation by implantation of oxygen) and bulk starting material. Four varieties were included in this study: bulk (5 mu m epi on n/sup +/), and SIMOX/SOI with three silicon-layer thicknesses (0.5 mu m, 0.75 mu m, and 1.0 mu m). This combination allows the assessment of three device structures: standard bulk devices, standard SOI devices (S/D contacting the buried oxide), and semi-bulk SOI devices which operate like bulk devices but are dielectrically isolated. All the SOI SRAMs were functional to the maximum temperature available, 300 degrees C. The bulk circuits also functioned at elevated temperatures, but lost functionality between 250 degrees C and 275 degrees C due to the rapidly increasing leakage current associated with the well junction. The synchronous access time increased approximately linearly with temperature for all devices, and was nearly twice the measured room-temperature value at 300 degrees C. Leakage current increased strongly with temperature for all devices, with the thin SOI devices having the least static current at the highest temperatures.<>
求助全文
通过发布文献求助,成功后即可免费获取论文全文。 去求助
来源期刊
自引率
0.00%
发文量
0
期刊最新文献
Ultra-thin high quality SOS films SOI thin film fully depleted high performance devices Silicon on SiO/sub 2/ by two step thermal bonding (TSTB) process Monitoring of heavy metals in as-implanted SIMOX with surface photovoltage Drain junction leakage current in SIMOX/MOSFETs
×
引用
GB/T 7714-2015
复制
MLA
复制
APA
复制
导出至
BibTeX EndNote RefMan NoteFirst NoteExpress
×
×
提示
您的信息不完整,为了账户安全,请先补充。
现在去补充
×
提示
您因"违规操作"
具体请查看互助需知
我知道了
×
提示
现在去查看 取消
×
提示
确定
0
微信
客服QQ
Book学术公众号 扫码关注我们
反馈
×
意见反馈
请填写您的意见或建议
请填写您的手机或邮箱
已复制链接
已复制链接
快去分享给好友吧!
我知道了
×
扫码分享
扫码分享
Book学术官方微信
Book学术文献互助
Book学术文献互助群
群 号:481959085
Book学术
文献互助 智能选刊 最新文献 互助须知 联系我们:info@booksci.cn
Book学术提供免费学术资源搜索服务,方便国内外学者检索中英文文献。致力于提供最便捷和优质的服务体验。
Copyright © 2023 Book学术 All rights reserved.
ghs 京公网安备 11010802042870号 京ICP备2023020795号-1