{"title":"Sn99Ag0.3Cu0.7–TiO2 composite solder joints and their influence on thermal parameters of power components","authors":"Adrian Pietruszka, Paweł Górecki, Agata Skwarek","doi":"10.1108/ssmt-03-2024-0016","DOIUrl":null,"url":null,"abstract":"<h3>Purpose</h3>\n<p>This paper aims to investigate the influence of composite solder joint preparation on the thermal properties of metal-oxide-semiconductor field-effect transistors (MOSFETs) and the mechanical strength of the soldered joint.</p><!--/ Abstract__block -->\n<h3>Design/methodology/approach</h3>\n<p>Reinforced composite solder joints with the addition of titanium oxide nanopowder (TiO<sub>2</sub>) were prepared. The reference alloy was Sn99Ag0.3Cu0.7. Reinforced joints differed in the weight percentage of TiO<sub>2</sub>, ranging from 0.125 to 1.0 Wt.%. Two types of components were used for the tests. The resistor in the 0805 package was used for mechanical strength tests, where the component was soldered to the FR4 substrate. For thermal parameters measurements, a power element MOSFET in a TO-263 package was used, which was soldered to a metal core printed circuit board (PCB) substrate. Components were soldered in batch IR oven.</p><!--/ Abstract__block -->\n<h3>Findings</h3>\n<p>Shear tests showed that the addition of titanium oxide does not significantly increase the resistance of the solder joint to mechanical damage. Titanium oxide addition was shown to not considerably influence the soldered joint’s mechanical strength compared to reference samples when soldered in batch ovens. Thermal resistance <em>R<sub>thj-a</sub></em> of MOSFETs depends on TiO<sub>2</sub> concentration in the composite solder joint reaching the minimum <em>R<sub>thj</sub></em> at 0.25 Wt.% of TiO<sub>2</sub>.</p><!--/ Abstract__block -->\n<h3>Research limitations/implications</h3>\n<p>Mechanical strength: TiO<sub>2</sub> reinforcement shows minimal impact on mechanical strength, suggesting altered liquidus temperature and microstructure, requiring further investigation. Thermal performance: thermal parameters vary with TiO<sub>2</sub> concentration, with optimal performance at 0.25 Wt.%. Experimental validation is crucial for practical application. Experimental confirmation: validation of optimal concentrations is essential for accurate assessment and real-world application. Soldering method influence: batch oven soldering may affect mechanical strength, necessitating exploration of alternative methods. Thermal vs mechanical enhancement: while TiO<sub>2</sub> does not notably enhance mechanical strength, it improves thermal properties, highlighting the need for balanced design in power semiconductor assembly.</p><!--/ Abstract__block -->\n<h3>Practical implications</h3>\n<p>Incorporating TiO<sub>2</sub> enhances thermal properties in power semiconductor assembly. Optimal concentration balancing thermal performance and mechanical strength must be determined experimentally. Batch oven soldering may influence mechanical strength, requiring evaluation of alternative techniques. TiO<sub>2</sub> composite solder joints offer promise in power electronics for efficient heat dissipation. Microstructural analysis can optimize solder joint design and performance. Rigorous quality control during soldering ensures consistent thermal performance and mitigates negative effects on mechanical strength.</p><!--/ Abstract__block -->\n<h3>Social implications</h3>\n<p>The integration of TiO<sub>2</sub> reinforcement in solder joints impacts thermal properties crucial for power semiconductor assembly. However, its influence on mechanical strength is limited, potentially affecting product reliability. Understanding these effects necessitates collaborative efforts between researchers and industry stakeholders to develop robust soldering techniques. Ensuring optimal TiO<sub>2</sub> concentration through experimental validation is essential to maintain product integrity and safety standards. Additionally, dissemination of research findings and best practices can empower manufacturers to make informed decisions, fostering innovation and sustainability in electronic manufacturing processes. Ultimately, addressing these social implications promotes technological advancement while prioritizing consumer trust and product quality in the electronics industry.</p><!--/ Abstract__block -->\n<h3>Originality/value</h3>\n<p>The research shows the importance of the soldering technology used to assemble MOSFET devices.</p><!--/ Abstract__block -->","PeriodicalId":49499,"journal":{"name":"Soldering & Surface Mount Technology","volume":"18 1","pages":""},"PeriodicalIF":1.7000,"publicationDate":"2024-07-09","publicationTypes":"Journal Article","fieldsOfStudy":null,"isOpenAccess":false,"openAccessPdf":"","citationCount":"0","resultStr":null,"platform":"Semanticscholar","paperid":null,"PeriodicalName":"Soldering & Surface Mount Technology","FirstCategoryId":"88","ListUrlMain":"https://doi.org/10.1108/ssmt-03-2024-0016","RegionNum":4,"RegionCategory":"材料科学","ArticlePicture":[],"TitleCN":null,"AbstractTextCN":null,"PMCID":null,"EPubDate":"","PubModel":"","JCR":"Q3","JCRName":"ENGINEERING, ELECTRICAL & ELECTRONIC","Score":null,"Total":0}
引用次数: 0
Abstract
Purpose
This paper aims to investigate the influence of composite solder joint preparation on the thermal properties of metal-oxide-semiconductor field-effect transistors (MOSFETs) and the mechanical strength of the soldered joint.
Design/methodology/approach
Reinforced composite solder joints with the addition of titanium oxide nanopowder (TiO2) were prepared. The reference alloy was Sn99Ag0.3Cu0.7. Reinforced joints differed in the weight percentage of TiO2, ranging from 0.125 to 1.0 Wt.%. Two types of components were used for the tests. The resistor in the 0805 package was used for mechanical strength tests, where the component was soldered to the FR4 substrate. For thermal parameters measurements, a power element MOSFET in a TO-263 package was used, which was soldered to a metal core printed circuit board (PCB) substrate. Components were soldered in batch IR oven.
Findings
Shear tests showed that the addition of titanium oxide does not significantly increase the resistance of the solder joint to mechanical damage. Titanium oxide addition was shown to not considerably influence the soldered joint’s mechanical strength compared to reference samples when soldered in batch ovens. Thermal resistance Rthj-a of MOSFETs depends on TiO2 concentration in the composite solder joint reaching the minimum Rthj at 0.25 Wt.% of TiO2.
Research limitations/implications
Mechanical strength: TiO2 reinforcement shows minimal impact on mechanical strength, suggesting altered liquidus temperature and microstructure, requiring further investigation. Thermal performance: thermal parameters vary with TiO2 concentration, with optimal performance at 0.25 Wt.%. Experimental validation is crucial for practical application. Experimental confirmation: validation of optimal concentrations is essential for accurate assessment and real-world application. Soldering method influence: batch oven soldering may affect mechanical strength, necessitating exploration of alternative methods. Thermal vs mechanical enhancement: while TiO2 does not notably enhance mechanical strength, it improves thermal properties, highlighting the need for balanced design in power semiconductor assembly.
Practical implications
Incorporating TiO2 enhances thermal properties in power semiconductor assembly. Optimal concentration balancing thermal performance and mechanical strength must be determined experimentally. Batch oven soldering may influence mechanical strength, requiring evaluation of alternative techniques. TiO2 composite solder joints offer promise in power electronics for efficient heat dissipation. Microstructural analysis can optimize solder joint design and performance. Rigorous quality control during soldering ensures consistent thermal performance and mitigates negative effects on mechanical strength.
Social implications
The integration of TiO2 reinforcement in solder joints impacts thermal properties crucial for power semiconductor assembly. However, its influence on mechanical strength is limited, potentially affecting product reliability. Understanding these effects necessitates collaborative efforts between researchers and industry stakeholders to develop robust soldering techniques. Ensuring optimal TiO2 concentration through experimental validation is essential to maintain product integrity and safety standards. Additionally, dissemination of research findings and best practices can empower manufacturers to make informed decisions, fostering innovation and sustainability in electronic manufacturing processes. Ultimately, addressing these social implications promotes technological advancement while prioritizing consumer trust and product quality in the electronics industry.
Originality/value
The research shows the importance of the soldering technology used to assemble MOSFET devices.
期刊介绍:
Soldering & Surface Mount Technology seeks to make an important contribution to the advancement of research and application within the technical body of knowledge and expertise in this vital area. Soldering & Surface Mount Technology compliments its sister publications; Circuit World and Microelectronics International.
The journal covers all aspects of SMT from alloys, pastes and fluxes, to reliability and environmental effects, and is currently providing an important dissemination route for new knowledge on lead-free solders and processes. The journal comprises a multidisciplinary study of the key materials and technologies used to assemble state of the art functional electronic devices. The key focus is on assembling devices and interconnecting components via soldering, whilst also embracing a broad range of related approaches.